I bought one for $150 with shipping. Once I use up the two carts it came with I may swap the electronics depending on the quality I get as it is. The carts are still $60 each and hold a 3rd of what you get in bulk. So hacking or converting is a necessary step with these.
I do have a question to those that have one. Mine was shipped with 1000 adhesion slides which are basically microscope slides and the seller claims they are needed and is included as a freebie. Most units don't include but need them according to the seller. However I can find no mention of them in the manual nor have I heard of a need for them in my years of printing. So what are they for or is the seller just shipping extra junk to get rid of it?
EDIT:
Got it running stock right now and these things are noisy.. Sounds like they are over driving the steppers like XYZ did.
Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.