Topic: FilaStruder, temp drops over 30C as soon as motors (and fans) turn on
Hi, this is my first post, was wondering if someone has ever encountered this issue, or know the common solutions to this kind of issue.
I got the Filastruder all wired up, turned on the main switch to get the heating going, and I also auto tuned the PID, and changed the CTRL thing to 2, and it heated up to the desired temp (180C) which was perfect. Then I turned on the Filastruder and after a few minutes a stream of ABS plastic was flowing out, however when I checked the temp, I noticed it started to drop down to 160c's then 150cs and stood around there, and the motor also started to have a harder time pushing the filament.
Has anyone ever encountered this issue?