Topic: Y shift 9 hours in!!
I got pretty confident with how things were running, so I tried the largest print I have done yet on my month old Da Vinci 1.0a, Repetier FW 0.92 running on Octoprint server on Raspberry Pi B+
130 x 84 x 135, 10% infill, 13 hour print.
About 8 hours in, I had a massive shift in the y axis toward the front of the printer. From that point up it seems to be fine.
Frustrating to say the least.
Luckily, I think I will be able to take a scalpel and de-laminate the entire layer and reattach it.
But what a slap in the face after 9 hours of beautiful print.
I checked the bed to make sure it is not loose. I checked the filament to make sure it wasn't caught up. The stepper motors didn't seem too hot.
Is this just an occasional plague with longer prints?