Topic: Using concentrated ABS solution/ ABS powder
Hi I am trying to do some experiments here.
Just want to check if you guys advise against using concentrated ABS solution instead of pellets, and what is expected to happen if I do that.
(I assume it is not advised) Then will it be better if I let it evaporate and cut the residue chunk into pieces then put inside?
On the other hand, how about ABS powder instead of pellets?