Here my settings:


[filament:eSUN PLA]
bed_temperature = 55
bridge_fan_speed = 100
cooling = 0
disable_fan_first_layers = 1
extrusion_multiplier = 0.935
fan_always_on = 1
fan_below_layer_time = 60
filament_colour = #000000
filament_diameter = 1.75
first_layer_bed_temperature = 55
first_layer_temperature = 205
max_fan_speed = 100
min_fan_speed = 100
min_print_speed = 10
slowdown_below_layer_time = 30
temperature = 205

[presets]
filament = eSUN PLA.ini
print = Medium.ini
printer = 40 4.ini


[print:Medium speed]
avoid_crossing_perimeters = 1
bottom_solid_layers = 4
bridge_acceleration = 0
bridge_flow_ratio = 1
bridge_speed = 20
brim_width = 0
complete_objects = 0
default_acceleration = 0
dont_support_bridges = 0
external_fill_pattern = rectilinear
external_perimeter_extrusion_width = 0
external_perimeter_speed = 80%
external_perimeters_first = 0
extra_perimeters = 1
extruder_clearance_height = 20
extruder_clearance_radius = 20
extrusion_width = 0
fill_angle = 45
fill_density = 0%
fill_pattern = rectilinear
first_layer_acceleration = 0
first_layer_extrusion_width = 200%
first_layer_height = 0.3
first_layer_speed = 20%
gap_fill_speed = 40
gcode_comments = 0
infill_acceleration = 0
infill_every_layers = 1
infill_extruder = 1
infill_extrusion_width = 0
infill_first = 0
infill_only_where_needed = 0
infill_overlap = 15%
infill_speed = 70
interface_shells = 0
layer_height = 0.3
max_print_speed = 80
max_volumetric_speed = 0
min_skirt_length = 10
notes =
only_retract_when_crossing_perimeters = 0
ooze_prevention = 0
output_filename_format = [input_filename_base].gcode
overhangs = 1
perimeter_acceleration = 0
perimeter_extruder = 1
perimeter_extrusion_width = 0
perimeter_speed = 60
perimeters = 2
post_process =
raft_layers = 0
resolution = 0
seam_position = aligned
skirt_distance = 2
skirt_height = 1
skirts = 1
small_perimeter_speed = 70%
solid_infill_below_area = 70
solid_infill_every_layers = 0
solid_infill_extruder = 1
solid_infill_extrusion_width = 0
solid_infill_speed = 80%
spiral_vase = 0
standby_temperature_delta = -5
support_material = 0
support_material_angle = 0
support_material_contact_distance = 0.2
support_material_enforce_layers = 0
support_material_extruder = 1
support_material_extrusion_width = 0
support_material_interface_extruder = 1
support_material_interface_layers = 3
support_material_interface_spacing = 0
support_material_interface_speed = 75%
support_material_pattern = honeycomb
support_material_spacing = 10
support_material_speed = 40
support_material_threshold = 10
thin_walls = 1
threads = 8
top_infill_extrusion_width = 0
top_solid_infill_speed = 30
top_solid_layers = 4
travel_speed = 130
xy_size_compensation = 0

[printer:40 4]
bed_shape = 0x0,200x0,200x200,0x200
before_layer_gcode =
end_gcode = M104 S0 ; turn off temperature\nG28 X0  ; home X axis\nM84     ; disable motors\n
extruder_offset = 0x0
gcode_flavor = reprap
layer_gcode =
nozzle_diameter = 0.4
octoprint_apikey =
octoprint_host =
pressure_advance = 0
retract_before_travel = 1.5
retract_layer_change = 1
retract_length = 4
retract_length_toolchange = 10
retract_lift = 0
retract_restart_extra = 0
retract_restart_extra_toolchange = 0
retract_speed = 40
start_gcode = G28 ; home all axes\nG1 Z5 F5000 ; lift nozzle\n
toolchange_gcode =
use_firmware_retraction = 0
use_relative_e_distances = 0
use_volumetric_e = 0
vibration_limit = 0
wipe = 0
z_offset = 0

Post's attachments

IMG_0079.JPG
IMG_0079.JPG 1.92 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
Da Vinci 1.0A Blue | Codename: FreeVinci | E3D v6 Bowden Custom Carriage | Printing PLA, ABS and PETG using S3D
Fabrikator Mini Orange | Printing PLA using Cura
Only printing with sub 20 Euro filaments.

2

Re: What causes this line?

My first bet is that your seam position (layer changes) are aligned...but it does not go all the way to the bottom which is strange...if that is the seam position, try randomizing it and/or increasing your retraction.

SD2 - Stock - Enclosure - Heated Bed - Glass Plate - Auto Fire Extinguisher
Ord Bot Hadron - RAMPS 1.4 - Bulldog XL - E3D v6 - 10" x 10" PCB Heated Build w/SSR - Glass Plate
Thanks for All of Your Help!

3

Re: What causes this line?

I tryed to randomize it but it gave me blobs everywhere.

Da Vinci 1.0A Blue | Codename: FreeVinci | E3D v6 Bowden Custom Carriage | Printing PLA, ABS and PETG using S3D
Fabrikator Mini Orange | Printing PLA using Cura
Only printing with sub 20 Euro filaments.

4

Re: What causes this line?

Instead of blobs all in one line smile

So make sure "Retract on Layer Change" is enabled; and try increasing the retraction amount if necessary.