		<title><![CDATA[SoliForum - 3D Printing Community — What causes this line?]]></title>
		<link>https://www.soliforum.com/topic/14259/what-causes-this-line/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/14259/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in What causes this line?.]]></description>
		<lastBuildDate>Wed, 09 Mar 2016 21:52:18 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: What causes this line?]]></title>
			<link>https://www.soliforum.com/post/118999/#p118999</link>
			<description><![CDATA[<p>Instead of blobs all in one line <img src="https://www.soliforum.com/img/smilies/smile.png" width="15" height="15" alt="smile" /></p><p>So make sure &quot;Retract on Layer Change&quot; is enabled; and try increasing the retraction amount if necessary.</p>]]></description>
			<author><![CDATA[null@example.com (IronMan)]]></author>
			<pubDate>Wed, 09 Mar 2016 21:52:18 +0000</pubDate>
			<guid>https://www.soliforum.com/post/118999/#p118999</guid>
		</item>
		<item>
			<title><![CDATA[Re: What causes this line?]]></title>
			<link>https://www.soliforum.com/post/118997/#p118997</link>
			<description><![CDATA[<p>I tryed to randomize it but it gave me blobs everywhere.</p>]]></description>
			<author><![CDATA[null@example.com (DopeSkrit)]]></author>
			<pubDate>Wed, 09 Mar 2016 21:45:15 +0000</pubDate>
			<guid>https://www.soliforum.com/post/118997/#p118997</guid>
		</item>
		<item>
			<title><![CDATA[Re: What causes this line?]]></title>
			<link>https://www.soliforum.com/post/118996/#p118996</link>
			<description><![CDATA[<p>My first bet is that your seam position (layer changes) are aligned...but it does not go all the way to the bottom which is strange...if that is the seam position, try randomizing it and/or increasing your retraction.</p>]]></description>
			<author><![CDATA[null@example.com (IronMan)]]></author>
			<pubDate>Wed, 09 Mar 2016 21:39:13 +0000</pubDate>
			<guid>https://www.soliforum.com/post/118996/#p118996</guid>
		</item>
		<item>
			<title><![CDATA[What causes this line?]]></title>
			<link>https://www.soliforum.com/post/118995/#p118995</link>
			<description><![CDATA[<p>What causes this line?</p><p>Here my settings:</p><br /><p>[filament:eSUN PLA]<br />bed_temperature = 55<br />bridge_fan_speed = 100<br />cooling = 0<br />disable_fan_first_layers = 1<br />extrusion_multiplier = 0.935<br />fan_always_on = 1<br />fan_below_layer_time = 60<br />filament_colour = #000000<br />filament_diameter = 1.75<br />first_layer_bed_temperature = 55<br />first_layer_temperature = 205<br />max_fan_speed = 100<br />min_fan_speed = 100<br />min_print_speed = 10<br />slowdown_below_layer_time = 30<br />temperature = 205</p><p>[presets]<br />filament = eSUN PLA.ini<br />print = Medium.ini<br />printer = 40 4.ini</p><br /><p>[print:Medium speed]<br />avoid_crossing_perimeters = 1<br />bottom_solid_layers = 4<br />bridge_acceleration = 0<br />bridge_flow_ratio = 1<br />bridge_speed = 20<br />brim_width = 0<br />complete_objects = 0<br />default_acceleration = 0<br />dont_support_bridges = 0<br />external_fill_pattern = rectilinear<br />external_perimeter_extrusion_width = 0<br />external_perimeter_speed = 80%<br />external_perimeters_first = 0<br />extra_perimeters = 1<br />extruder_clearance_height = 20<br />extruder_clearance_radius = 20<br />extrusion_width = 0<br />fill_angle = 45<br />fill_density = 0%<br />fill_pattern = rectilinear<br />first_layer_acceleration = 0<br />first_layer_extrusion_width = 200%<br />first_layer_height = 0.3<br />first_layer_speed = 20%<br />gap_fill_speed = 40<br />gcode_comments = 0<br />infill_acceleration = 0<br />infill_every_layers = 1<br />infill_extruder = 1<br />infill_extrusion_width = 0<br />infill_first = 0<br />infill_only_where_needed = 0<br />infill_overlap = 15%<br />infill_speed = 70<br />interface_shells = 0<br />layer_height = 0.3<br />max_print_speed = 80<br />max_volumetric_speed = 0<br />min_skirt_length = 10<br />notes = <br />only_retract_when_crossing_perimeters = 0<br />ooze_prevention = 0<br />output_filename_format = [input_filename_base].gcode<br />overhangs = 1<br />perimeter_acceleration = 0<br />perimeter_extruder = 1<br />perimeter_extrusion_width = 0<br />perimeter_speed = 60<br />perimeters = 2<br />post_process = <br />raft_layers = 0<br />resolution = 0<br />seam_position = aligned<br />skirt_distance = 2<br />skirt_height = 1<br />skirts = 1<br />small_perimeter_speed = 70%<br />solid_infill_below_area = 70<br />solid_infill_every_layers = 0<br />solid_infill_extruder = 1<br />solid_infill_extrusion_width = 0<br />solid_infill_speed = 80%<br />spiral_vase = 0<br />standby_temperature_delta = -5<br />support_material = 0<br />support_material_angle = 0<br />support_material_contact_distance = 0.2<br />support_material_enforce_layers = 0<br />support_material_extruder = 1<br />support_material_extrusion_width = 0<br />support_material_interface_extruder = 1<br />support_material_interface_layers = 3<br />support_material_interface_spacing = 0<br />support_material_interface_speed = 75%<br />support_material_pattern = honeycomb<br />support_material_spacing = 10<br />support_material_speed = 40<br />support_material_threshold = 10<br />thin_walls = 1<br />threads = 8<br />top_infill_extrusion_width = 0<br />top_solid_infill_speed = 30<br />top_solid_layers = 4<br />travel_speed = 130<br />xy_size_compensation = 0</p><p>[printer:40 4]<br />bed_shape = 0x0,200x0,200x200,0x200<br />before_layer_gcode = <br />end_gcode = M104 S0 ; turn off temperature\nG28 X0&nbsp; ; home X axis\nM84&nbsp; &nbsp; &nbsp;; disable motors\n<br />extruder_offset = 0x0<br />gcode_flavor = reprap<br />layer_gcode = <br />nozzle_diameter = 0.4<br />octoprint_apikey = <br />octoprint_host = <br />pressure_advance = 0<br />retract_before_travel = 1.5<br />retract_layer_change = 1<br />retract_length = 4<br />retract_length_toolchange = 10<br />retract_lift = 0<br />retract_restart_extra = 0<br />retract_restart_extra_toolchange = 0<br />retract_speed = 40<br />start_gcode = G28 ; home all axes\nG1 Z5 F5000 ; lift nozzle\n<br />toolchange_gcode = <br />use_firmware_retraction = 0<br />use_relative_e_distances = 0<br />use_volumetric_e = 0<br />vibration_limit = 0<br />wipe = 0<br />z_offset = 0</p>]]></description>
			<author><![CDATA[null@example.com (DopeSkrit)]]></author>
			<pubDate>Wed, 09 Mar 2016 21:09:44 +0000</pubDate>