1 (edited by salmanilla 2016-02-24 16:10:45)

Topic: Having Issues with Repetier Software and the Davinci 1.0A

I am having some bizarre problems with my DaVinci Printer after installing the Repetier Firmware.  I am sure that it is some type of configuration problem...  Just not sure where to begin in correcting the issue.  Please look at image attached.

-Sal-

Post's attachments

3D Printer.jpg
3D Printer.jpg 225.04 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.

2

Re: Having Issues with Repetier Software and the Davinci 1.0A

Looks like poor bed adhesion. Adjust your nozzle height properly and use glue stick.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Having Issues with Repetier Software and the Davinci 1.0A

Is it possible that the Extruder Temp I am using is incorrect?  I am using 200c with Standard Davinci ABS Filament 1.75...  Bed Temp of 110.

-Sal-

4

Re: Having Issues with Repetier Software and the Davinci 1.0A

ABS is normally in the 235 range. Your image however is what happens when the base of your print comes free and the printer then just prints in the air. So your bed adhesion and maybe first layer quality is bad.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.