Topic: ABS + Copper and ABS + Iron filament production
Lots of folks have asked if it is possible to replicate Copper-filled and Iron-filled filaments with a Filastruder. Turns out the answer is yes!
https://www.researchgate.net/profile/Ra … 07e693.pdf
Here's a teaser photo from the paper, copper filled ABS: