Topic: Wired E3D v6 jamming issue after printing PMMA filament
So I recently picked up a roll of PMMA Filament (https://en.wikipedia.org/wiki/Poly%28me … crylate%29) after printing some test prints I wanted to switch back to my usual PLA and it jammed sometimes but sometimes it worked. After heating up my hotend to 250 and extruding 5m of PLA plastic it worked again (I unloaded the PLA 4 times at 90°C). Have somebody exprienced similar issues when printing high temp plastics with the v6?
Fabrikator Mini Orange | Printing PLA using Cura
Only printing with sub 20 Euro filaments.