Topic: calibrated steps/mm and extrusion multiplier... but overextrudes fill
I recently installed e3d on my SD2 and have ironed almost all kinks.
The latest is that when I do .4 infill, it overextrudes and looks like this: https://www.simplify3d.com/support/prin … ch-plastic
It shouldn't. I've done 40% infill before and that didn't happen.
I have calibrated steps/mm and set it in firmware. I have tested a single walled print and set the extrusion multipler (to 0.99, miraculously).
I have entered an average of measurements of the filament diameter.
My e3d tip is .4mm, and my layer height is .3, extrusion width 0.42. I've read this might be wrong but I can't seem to find a guide to the relationship with the larger tip.
Printing at 230 (e3d's thermistor).
Any thoughts / help?