Topic: Best prices for ABS Pellets?

I need some more ABS pellets and haven't bought any since OSPrinting a long time ago.

Anybody have recommendations beyond (or amongst) the ones listed on the pinned page to get them cheaply? The going rate seems to be about or above $5 per pound, which is higher than I was hoping for.  With 2.2lb spools of finished filament now selling on Amazon for $20 shipped, the cost/benefit comparison isn't nearly as compelling as it once was, especially if I need to extrude twice to get uniform filament.

2

Re: Best prices for ABS Pellets?

$2/pound shipped on eBay if you know what you're looking for:

http://www.ebay.com/itm/20-lb-Virgin-AB … SwLVZV2kyW

PA-746 is fairly common in filament.

Do keep in mind also that Sabic MG94 at $5/pound is going to be better quality than the $20 Amazon stuff.

3

Re: Best prices for ABS Pellets?

elmoret wrote:

$2/pound shipped on eBay if you know what you're looking for:

Perfect!  That's exactly what I needed, (as I obviously don't know what I'm looking for).

I got burned previously ordering some "virgin black abs for injection molding" without requesting specs and found it didn't extrude well at all (brittle and super slow extrusion at 180).  Besides MG-94 and PA-746, is there anything else I be on the look out for?

4

Re: Best prices for ABS Pellets?

Googling the resin ID and comparing the MFR are a good first step.

5

Re: Best prices for ABS Pellets?

Hah!  I looked again at what I ordered.  I missed that it as listed as PC ABS, a polycarbonite/ABS blend.  The processing temp is listed at 475-525 F (246-274 C).  No wonder I couldn't extrude it!

6

Re: Best prices for ABS Pellets?

I ordered the above... I am getting excruciatingly slow extrusion at maybe 6 inch a minute. Ive tried 180-200 degrees to get 1.65mm

elmoret wrote:

$2/pound shipped on eBay if you know what you're looking for:

http://www.ebay.com/itm/20-lb-Virgin-AB … SwLVZV2kyW

PA-746 is fairly common in filament.

Do keep in mind also that Sabic MG94 at $5/pound is going to be better quality than the $20 Amazon stuff.

7

Re: Best prices for ABS Pellets?

You might want to check your setup (clean melt filter nozzle, etc) as someone just reported 21"/minute with that material:

http://www.soliforum.com/topic/13811/abs-pa746/