Does anyone have a source for new rods mine have managed to get corroded and are now causing problems. my nephew dropped some water on them grr
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Help/Repair/Maintenance → replacing rods for sd3
Does anyone have a source for new rods mine have managed to get corroded and are now causing problems. my nephew dropped some water on them grr
http://www.mcmaster.com/#linear-shafts/=10qj4dz
http://folger-technologies-llc.myshopif … ter-cnc-o1
Much cheaper than McMaster and these are also good quality, I have them on my printer. You will need a dremel with cutting wheel to trim them to size. Also, you will want to upgrade to linear bearings with Lawsy carriages at the same time, the stock bushings will not work well on these. But if you must stick with the stock bushings, I have the old SD3 stock rods that I could sell you for cost of shipping. But don't do that, the smooth rods with bearings are a great upgrade.