1

Topic: Afinia H800 nozzel problems

I have been using the Afinia H800 for a few months now and just cant seem to get it to work with other filaments. I have had some success with the Hatchbox brand. I just installed the Octave temp switch and have done some test prints. Only problem is i get about 75% of the way through the prints and then the nozzle jams or something. I am using the recommended temps and the part that prints come out very nice. The raft comes off easy. it looks like the nozzle jams up. I withdraw the filament and try again with the same result. Any advice on this would be very appreciated. I want to be able to use other filaments without this problem.

2

Re: Afinia H800 nozzel problems

Try increasing temps in increments if 5.

Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions