Topic: What am I doing wrong??
I don't know what else to do. I have had my DaVinci since Christmas 2014 and have not used it much since it is so frustrating to get good results. I had it dialed in OK about 6 months ago and now I would like to use it for a new project I am working on. A week ago I flashed it with Repetier .92 and I am very happy with the new freedom it allows me for control. However I have not had a successful print since I flashed it. Some of my issues could be attributed to my new filament as well. I am using a new roll of HATCHBOX ABS. These photos are of my last attempt at printing my E3D V6 mount I can not seem to get anything usable. Can anyone tell what is going on based on the pictures?
Here are my settings.
Print Speed 40
First Layer Speed 30
Perimeter 30
Infill 60
Layer Height .2
Shell Thickness .8
Infill Overlap 15%
Air Gap 0
Retraction Speed 40mm/s
Retraction Distance 4mm
Hot End Temp 230
Bed Temp 115
If there are any other settings that would help please let me know.