Re: Replacement Glass Bed?
Just a heads up.
I sell the glass / heater pre-assembled and I have shipped around the world including Australia without incident.
I'm using the Borosilicate glass which is flat and doesn't warp when heated. I use the same company that makes the heaters for the Da Vinci so they fit and work perfectly.
Probably seen it but here is the thread.
http://www.soliforum.com/topic/9642/da- … th-heater/