1

Topic: Heater cutting out mid print

I'm currently running repetier firmware w/an e3D V6 (with their thermistor and heater). I tried printing something today but about 4 hours into the print the hotend's temp fell to ~40C and just stripped the filament (so it stopped extruder). I figured it was a fluke so I retried the print (but I opened the back and had a fan blowing on the mobo to see if it was maybe overheating) and it again was fine for ~20 minutes but then the same thing happened. I then resoldered the heater cables to see if maybe the connection was bad, and now it doesn't heat up at all. I used a hair dryer on it and the temp did rise, so I think the thermistor is ok, but I have tried heating the hotend from the onboard menu and my computer with no luck. Did my heater just randomly die or am I missing something?

da Vinci 1.0
Repetier Firmware, E3D v6 Hot End
Successfully printed in: ABS, PLA, Ninjaflex, Nylon, and Woodfill

2

Re: Heater cutting out mid print

pbcrazy wrote:

I'm currently running repetier firmware w/an e3D V6 (with their thermistor and heater). I tried printing something today but about 4 hours into the print the hotend's temp fell to ~40C and just stripped the filament (so it stopped extruder). I figured it was a fluke so I retried the print (but I opened the back and had a fan blowing on the mobo to see if it was maybe overheating) and it again was fine for ~20 minutes but then the same thing happened. I then resoldered the heater cables to see if maybe the connection was bad, and now it doesn't heat up at all. I used a hair dryer on it and the temp did rise, so I think the thermistor is ok, but I have tried heating the hotend from the onboard menu and my computer with no luck. Did my heater just randomly die or am I missing something?


if you have a meter that can measure resistance, disconnect the heater and measure across it at it's leads and see what it measures.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Heater cutting out mid print

carl_m1968 wrote:

if you have a meter that can measure resistance, disconnect the heater and measure across it at it's leads and see what it measures.

Unfortunately I do not have a meter here.

da Vinci 1.0
Repetier Firmware, E3D v6 Hot End
Successfully printed in: ABS, PLA, Ninjaflex, Nylon, and Woodfill

4

Re: Heater cutting out mid print

Replaced the heater and all is good. It only had <20 hours on it, and from other forums it seems relatively normal for e3D heaters. But all is good again!

da Vinci 1.0
Repetier Firmware, E3D v6 Hot End
Successfully printed in: ABS, PLA, Ninjaflex, Nylon, and Woodfill