I have started using a glue that as far as I can see is the same as Elmers Purple Disappearing Glue. I can't get Elmers because they don't stock it in the UK but this stuff seems to be identical barring the text on the gluestick.

Anyway, it sticks the PLA print to the glass really well, no more curling... However getting it off can be a problem.

I have had some limited luck with tapping it off with the handle of a screwdriver but prints with a larger contact area with the glass get stuck hard. I have tried putting it (with the glass) in warm water overnight but with no luck and I poured 90 celcius water over it this morning to try to remove it but ended up warping the print.

Any better ideas? I have broken two glass plates so far and am going to go and buy a stock of them but obviously it would be better if I could just get the print off the glass reliably.

https://i.imgflip.com/sz7sa.jpgvia Imgflip Meme Maker

2

Re: Elmers Purple Disappearing Glue - print stuck hard to glass bed

Generic glue is fine. I use it all the time. It is all essentially the same stuff.

I occasionally have the same problem. If you have a removable glass plate (which it sounds like you do), the glue is made to wash off the hands of kids easily in the sink. Use warm water and the glue will turn purple again, and then eventually wash off. You can also wash the residue off the bottom of your print. Just don't make it too hot.

I also bought a 4" paint scraper. I will slide this under the corner of a print and gently work it until the print comes free. BE VERY CAREFUL! Without securing the glass, you do not want to cut your other arm. Sometimes when the prints are cool, I have to give a stiff, short jab at the base to get under the print. Sometimes they will pop clean off.

Additionally, if you use ABS and let it cool sufficiently, it will usually pop off on its own because it shrinks just a little as it cools.

Solidoodle 4-Mostly stock running off headless Raspberry Pi with Octoprint

3

Re: Elmers Purple Disappearing Glue - print stuck hard to glass bed

Try a misting of extra-hold hairspray instead. Will leave glassy finish and is easier to pop off.

FuseBox 1.5 CoreXY - e3dv6 - Graphic Smart Display
Solidoodle 2 - e3dv6 - Hobb Goblin - e3d Titan - lawsy carriages - Direct Drive Y Axis - T8 Z axis - OctoPi

4

Re: Elmers Purple Disappearing Glue - print stuck hard to glass bed

I just use a large Exacto knife shaped like a chisel. I git it under one corner then gradually slid it in further. The blade is thin enough it causes no warping. If I need to I will do the same on a different corner.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

5

Re: Elmers Purple Disappearing Glue - print stuck hard to glass bed

Widespread: I originally used this stuff...

https://i.imgflip.com/stug7.jpgvia Imgflip Meme Maker

but it was so strong it took a sliver of glass off with the print...

https://i.imgflip.com/su6h7.jpgvia Imgflip Meme Maker

https://i.imgflip.com/su6j3.jpgvia Imgflip Meme Maker

Morganism; Carl_m1968: Looks like I am going to get some sort of razor.

6

Re: Elmers Purple Disappearing Glue - print stuck hard to glass bed

i use single edge razors (bought a 100 pack at local home improvement store) to get under an edge or corner of a print to work it loose all the time - just use a bit of common sense with them - they are very sharp after all. =P

SD4 #1 & #2 - Lawsy carriages, E3D v6, Rumba controller board, mirror bed plate, X motor fan, upgraded PSU & Mica bed heater
SD4 #3 - in the works ~ Folgertech FT-5, rev 1
Printit Industries Beta Tester - Horizon H1

7

Re: Elmers Purple Disappearing Glue - print stuck hard to glass bed

heartless wrote:

i use single edge razors (bought a 100 pack at local home improvement store) to get under an edge or corner of a print to work it loose all the time - just use a bit of common sense with them - they are very sharp after all. =P

I use a razor on large prints too, but never had glass come off.

Are you using a lot of spray? You only need a quick once over or two, then let that dry. You don't need to mist every time, either.

FuseBox 1.5 CoreXY - e3dv6 - Graphic Smart Display
Solidoodle 2 - e3dv6 - Hobb Goblin - e3d Titan - lawsy carriages - Direct Drive Y Axis - T8 Z axis - OctoPi

8

Re: Elmers Purple Disappearing Glue - print stuck hard to glass bed

widespreaddeadhead wrote:

Are you using a lot of spray? You only need a quick once over or two, then let that dry. You don't need to mist every time, either.

^ this. A couple of light coats should be good for multiple prints. I usually do one light coat from side to side, let it set up, then another light coat front to back to ensure even coverage. one application will usually last me for nearly a week of heavy printing. when things start to not stick anymore, I clean it off with windex and start over

SD4 #1 & #2 - Lawsy carriages, E3D v6, Rumba controller board, mirror bed plate, X motor fan, upgraded PSU & Mica bed heater
SD4 #3 - in the works ~ Folgertech FT-5, rev 1
Printit Industries Beta Tester - Horizon H1