Topic: Print speed ... extruder limited ?
Hello,
I did some tests on the solidoodle over the last week ...
Doing speed test, my results are that the X/Y axes are very fast once setup correctly (I'm traveling at 20m/min without any problem), the Z is ok (not used that much) ... but the limiting factor seems to be the extruder, I tried to push the speed limit and at some point the travel speed is still perfect but the extruder doesn't grip the filament enough to push it through the nozzle (I'm running the nozzle at 205°C).
Am I right or is my extruder not setup correctly ?