Topic: what would cause this problem?
the front looks flawless at .1 but the back of this figure is a mess.
Thanks
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → what would cause this problem?
the front looks flawless at .1 but the back of this figure is a mess.
Thanks
I'm not sure if I would consider any of that 'flawless', but the model could have a hole in it (Run it through netfabb before printing)
sorry i meant the front is flawless compared to the back. also i already ran the model thru netfabb, which didnt indicate any problem with the model.
Looks to me like you need to adjust retraction a bit on layer change. And, if not already set, randomize your layer starting points.
Looks to me like you need to adjust retraction a bit on layer change. And, if not already set, randomize your layer starting points.
thanks for the tip
What layer height did you print that at? There is a lot of banding in it that should not be there. Also what temp was this printed at and what speed? It looks to me your temp was too low and the speed was fast in some areas. The hole looks like a place that was too hot too long and did not get enough filament due to poor flow caused by the hotend not being hot enough. The filament has a flat look when it should be glossy or semi glossy.
What layer height did you print that at? There is a lot of banding in it that should not be there. Also what temp was this printed at and what speed? It looks to me your temp was too low and the speed was fast in some areas. The hole looks like a place that was too hot too long and did not get enough filament due to poor flow caused by the hotend not being hot enough. The filament has a flat look when it should be glossy or semi glossy.
i printed it at .1
temp was set at 230
speed 30
On a Da Vinci i would not go below.15 on layer height. I have yet to see a stock Da Vinci do a good print at .1, I honestly don't think they can actually do it even though XYZ claims they can. I know mine never could till I replaced the controller.
On a Da Vinci i would not go below.15 on layer height. I have yet to see a stock Da Vinci do a good print at .1, I honestly don't think they can actually do it even though XYZ claims they can. I know mine never could till I replaced the controller.
ok i will try .2 and see how it comes out. thanks