<?xml version="1.0" encoding="utf-8"?>
<rss version="2.0" xmlns:atom="http://www.w3.org/2005/Atom">
	<channel>
		<title><![CDATA[SoliForum - 3D Printing Community — what would cause this problem?]]></title>
		<link>https://www.soliforum.com/topic/12541/what-would-cause-this-problem/</link>
		<atom:link href="https://www.soliforum.com/feed/rss/topic/12541/" rel="self" type="application/rss+xml" />
		<description><![CDATA[The most recent posts in what would cause this problem?.]]></description>
		<lastBuildDate>Wed, 14 Oct 2015 13:47:22 +0000</lastBuildDate>
		<generator>PunBB</generator>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107567/#p107567</link>
			<description><![CDATA[<div class="quotebox"><cite>carl_m1968 wrote:</cite><blockquote><p>On a Da Vinci i would not go below.15 on layer height. I have yet to see a stock Da Vinci do a good print at .1, I honestly don&#039;t think they can actually do it even though XYZ claims they can. I know mine never could till I replaced the controller.</p></blockquote></div><p>ok i will try .2 and see how it comes out. thanks</p>]]></description>
			<author><![CDATA[null@example.com (TheNeck)]]></author>
			<pubDate>Wed, 14 Oct 2015 13:47:22 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107567/#p107567</guid>
		</item>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107551/#p107551</link>
			<description><![CDATA[<p>On a Da Vinci i would not go below.15 on layer height. I have yet to see a stock Da Vinci do a good print at .1, I honestly don&#039;t think they can actually do it even though XYZ claims they can. I know mine never could till I replaced the controller.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Wed, 14 Oct 2015 06:35:53 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107551/#p107551</guid>
		</item>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107548/#p107548</link>
			<description><![CDATA[<div class="quotebox"><cite>carl_m1968 wrote:</cite><blockquote><p>What layer height did you print that at? There is a lot of banding in it that should not be there. Also what temp was this printed at and what speed? It looks to me your temp was too low and the speed was fast in some areas. The hole looks like a place that was too hot too long and did not get enough filament due to poor flow caused by the hotend not being hot enough. The filament has a flat look when it should be glossy or semi glossy.</p></blockquote></div><p>i printed it at .1<br />temp was set at 230<br />speed 30</p>]]></description>
			<author><![CDATA[null@example.com (TheNeck)]]></author>
			<pubDate>Wed, 14 Oct 2015 05:45:22 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107548/#p107548</guid>
		</item>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107545/#p107545</link>
			<description><![CDATA[<p>What layer height did you print that at? There is a lot of banding in it that should not be there. Also what temp was this printed at and what speed? It looks to me your temp was too low and the speed was fast in some areas. The hole looks like a place that was too hot too long and did not get enough filament due to poor flow caused by the hotend not being hot enough. The filament has a flat look when it should be glossy or semi glossy.</p>]]></description>
			<author><![CDATA[null@example.com (carl_m1968)]]></author>
			<pubDate>Wed, 14 Oct 2015 03:57:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107545/#p107545</guid>
		</item>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107544/#p107544</link>
			<description><![CDATA[<div class="quotebox"><cite>ggunners wrote:</cite><blockquote><p>Looks to me like you need to adjust retraction a bit on layer change. And, if not already set, randomize your layer starting points.</p></blockquote></div><p>thanks for the tip</p>]]></description>
			<author><![CDATA[null@example.com (TheNeck)]]></author>
			<pubDate>Wed, 14 Oct 2015 03:29:45 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107544/#p107544</guid>
		</item>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107496/#p107496</link>
			<description><![CDATA[<p>Looks to me like you need to adjust retraction a bit on layer change. And, if not already set, randomize your layer starting points.</p>]]></description>
			<author><![CDATA[null@example.com (ggunners)]]></author>
			<pubDate>Tue, 13 Oct 2015 20:06:10 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107496/#p107496</guid>
		</item>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107476/#p107476</link>
			<description><![CDATA[<p>sorry i meant the front is flawless compared to the back. also i already ran the model thru netfabb, which didnt indicate any problem with the model.</p>]]></description>
			<author><![CDATA[null@example.com (TheNeck)]]></author>
			<pubDate>Tue, 13 Oct 2015 15:38:08 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107476/#p107476</guid>
		</item>
		<item>
			<title><![CDATA[Re: what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107475/#p107475</link>
			<description><![CDATA[<p>I&#039;m not sure if I would consider any of that &#039;flawless&#039;, but the model could have a hole in it (Run it through netfabb before printing)</p>]]></description>
			<author><![CDATA[null@example.com (pbcrazy)]]></author>
			<pubDate>Tue, 13 Oct 2015 15:35:11 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107475/#p107475</guid>
		</item>
		<item>
			<title><![CDATA[what would cause this problem?]]></title>
			<link>https://www.soliforum.com/post/107470/#p107470</link>
			<description><![CDATA[<p>the front looks flawless at .1 but the back of this figure is a mess.<br /><span class="postimg"><img src="http://soliforum.com/i/?xkMaD7J.jpg" alt="http://soliforum.com/i/?xkMaD7J.jpg" /></span></p><p>Thanks</p>]]></description>
			<author><![CDATA[null@example.com (TheNeck)]]></author>
			<pubDate>Tue, 13 Oct 2015 14:35:07 +0000</pubDate>
			<guid>https://www.soliforum.com/post/107470/#p107470</guid>