any idea what would cause these marks? 
3D printer Noob.
Stock ABS filaments
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → help identifying marks on print
any idea what would cause these marks? 
Check your bed and make sure it has no Z wobble. The glass is usually loose and can slide sisde to side during prints. Shim it with paper between the glass edges and bed frame.
Check that the bearing mounts on the vertical smooth rods are not loos. Normally the glue they used for the bearing comes loose and allows the bearing to move around independent of the bed. Clean it best you can to remove oil and grease from the surface of the bearing and the surround supports and then glue with something like goop or other strong adhesive. Or like others did just shove an exacto blade between the bearing and the mount and then break the blade off.
SoliForum - 3D Printing Community → XYZ Printing DaVinci → help identifying marks on print
Powered by PunBB, supported by Informer Technologies, Inc.