Topic: This Stuff Will STICK TO YOUR PRINTER BED!
Hey everyone, in my quest to find anything that would stick the plastic to my kapton tape bed better, I came across something called Screen Printer's Adhesive. It's designed to be used on heated screen printing beds and is REALLY sticky.
I just tried it and it worked PERFECT!
The brandd I got was "TEX Flash" Screen Printer's Adhesive. It is distributed by GSG Distributing out of Tulsa OK, or Houston TX. I got it from a friend who owns a print shop here in Texas. So far I have had zero troubles with the print sticking to the bed...AND it seems very easy to remove the print once the job is done.
Just wanted to share that bit of info...:)
Kevin