So I monitored the temperature and didn't see any shift in temp. I replaced the nozzle neck and I am receiving a new nozzle today I might try. I lowered speeds and still have the same problems with any model I print. About an inch above the print I start to get lower extrusion amounts and this causes issues with the layer splits. It doesn't make sense that it is happening at a certain point.
Oh yea I calibrated my printer as well. For some reason I feel like the extrusion rate is low. But my s3d settings are a little higher than normal for extrusion rates.
.20 nozzle tip with .38 thickness and 1.10 multiplier
.10 layer height thickness.
15-20% infill
3 shells
I've never had to use a fan with PLA either so maybe layers aren't cooling? But I don't know why I would need a fan now?