1 (edited by efes 2015-07-19 22:42:02)

Topic: print part problem

hello

print this : http://www.thingiverse.com/thing:511668
top of the hole is not close?
please help !


http://nsa37.casimages.com/img/2015/07/20/150720124207313915.jpg


my setup simplify3d

http://nsa38.casimages.com/img/2015/07/20/150720123736992323.jpg

http://nsa38.casimages.com/img/2015/07/20/150720123737266726.jpg

http://nsa37.casimages.com/img/2015/07/20/150720123737725094.jpg

http://nsa37.casimages.com/img/2015/07/20/15072012373810521.jpg

http://nsa37.casimages.com/img/2015/07/20/150720123738453340.jpg

http://nsa38.casimages.com/img/2015/07/20/150720123738900333.jpg


thx help

Post's attachments

20150719_235848 [800x600].jpg
20150719_235848 [800x600].jpg 85.42 kb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
davinci 1.0
firmware repetier

2

Re: print part problem

hello

normal dimension 9.60 i have 5.90 ....
problem davinci or .... my setup ?

http://nsa37.casimages.com/img/2015/07/20/150720111404101002.jpg

davinci 1.0
firmware repetier

3

Re: print part problem

I get it!
head extruder completely blocked !!!!
I do not know why?
I completely disassemble clean ....

http://soliforum.com/i/?E6EBVti.jpg

What is this glue on the thermistor?

thx

davinci 1.0
firmware repetier

4

Re: print part problem

It is high temperature epoxy, only way to remove it is carefully chip at it with something without damaging the thermistor or it's wires. It might also dissolve in acetone if you take the extruder apart and soak the heat block in acetone.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

5

Re: print part problem

this http://www.aliexpress.com/item/Free-shi … 75713.html good ?

davinci 1.0
firmware repetier

6

Re: print part problem

It is not that. If you want something to replace it with, just use high temperature rtv.


http://www.amazon.com/Permatex-81160-Hi … B0002UEN1A