Topic: pellets vs rolls
Is 10lbs of pellets equal to about 4.5 rolls of filament ? Is that a correct assumption?
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Filastruder → pellets vs rolls
Is 10lbs of pellets equal to about 4.5 rolls of filament ? Is that a correct assumption?
At 1 kilo spools, that's about right.
Yup, it is a constant mass process. Mass of pellets in = mass of filament out*.
This is a surprisingly frequent question, actually.
*like 0.0001% of the mass of pellets gets converted to volatiles during extrusion
thanks, do you have recommended pellet supplier?
Yes indeed, stickied in this very forum.