Topic: PLA and humidity
Hi,
I succeeded in extruding the ABS sample that came with the filastuder.
Happy, I try the PLA waste that I have and that's the big surprise. Large patties come out of the filastruder.
I think it's due to the humidity. He is at 35%. What maximum rate do you recommend to me?