Topic: PLA and humidity

Hi,

I succeeded in extruding the ABS sample that came with the filastuder.

Happy, I try the PLA waste that I have and that's the big surprise. Large patties come out of the filastruder. yikes

I think it's due to the humidity. He is at 35%. What maximum rate do you recommend to me?

Thanks in advance.