I used the CW from the wiki that is preset for the D7. It has boxes X and Y under image reflection checked. That may solve your orientation issue.
Are you setting CW to add a base to the model for adhesion? If so you need to have the model sunk into it by a few layers and then when the print is complete an cured you will have to cut and sand it down.
Or you need to print the model directly to the platform with build platform with no adhesion aids.
It looks like your print is separating after the base is printed. This leads me to think you raised your model x height and then created a base with same X height.
In your CW screen shot your curing times are way off. Your bottom exposure is set for 4000 ms that is only 4 seconds. It should be around 20 seconds or so which would be 20000. Your exposure time for other layers is also wrong. You have it set to 10 that is not seconds, but ms. So you are only curing for .01 seconds on your other layers. If you want 10 seconds then it needs to be set to 10000. Remember the setting is expecting ms as in microseconds not seconds. So you have to multiple times 1000 for seconds.
In summary bottom layers need long exposure of around 20 seconds or 20000 ms.
Other layers need exposure time of around 6 seconds or 6000 ms.
Your model in question should take around 3+ hours to complete.
Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.