My printer : Solidoodle 2 Pro, fully enclosed
Brand : Sainsmart
Color : White, Purple, Green
Material : ABS
Bed Temp : 90
Extruder Temp : 205
Extrusion Multiplier : 0.7
Grade of Print : A
perfect prints
Brand : MonoPrice
Material : ABS
Color : White Black
Bed Temp : 90
Extruder Temp : 205
Extrusion Multiplier : 0.7
Grade of Print : A
perfect prints, this is my favorite brand right now (1.26.2013)
Brand : MonoPrice
Material : PLA
Color : Red
Bed Temp :60
Extruder Temp : 175
Extrusion Multiplier : 0.7
Grade of Print : D
Good prints until clogging, have not tried again
Brand : KBell
Material : ABS
Color : Pink
Bed Temp : 90
Extruder Temp : 205
Extrusion Multiplier : 0.7
Grade of Print : C
ok prints on smaller items, some layer adhesion issues and stringiness, not usable for large prints
Brand : KBell
Material : ABS
Color : Orange, Tansparent
Bed Temp : 90
Extruder Temp : 190- 210
Extrusion Multiplier : 0.7 - 1.1
Grade of Print : F
unable to make it work get 5 good layers at best before it starts stripping and balling up
Brand : Solidoodle
Material : ABS
Color : White
Bed Temp : 90
Extruder Temp : 205
Extrusion Multiplier : 0.7
Grade of Print : A
Brand : Solidoodle
Material : ABS
Color : Blue
Bed Temp : 90
Extruder Temp : 205
Extrusion Multiplier : 0.7
Grade of Print : C
Layer Adhesion, stringing, brittle prints
Brand : FavePrices(ebay)
Material : ABS
Color : Sliver
Bed Temp : 90
Extruder Temp : 205
Extrusion Multiplier : 1.0
Grade of Print : B+
I print this material at 80% Flowrate !!!!
I have had some very good prints from this ABS, but the filament does have some thin spots, they are minor, but on a smooth surface print they became very noticeable.