Hi,

I would like to know what minimum distance you put between the two devices? I have filament distortion due to vibrations when I take the filament.

Thank you.

2

Re: Distance between filastruder & filawinder

I have had good results with mine set like this: Mine seems different than most, but it works for me.

Center of Fillastruder nozzle to center of Filawinder pickup tube you feed filament into - about 22.5"
Bottom of Filastruder nozzle about level with Filawinder pickup tube platform
Laser pickup sits on a table 16" below nozzle.
I will post some pics shortly.

3

Re: Distance between filastruder & filawinder

Hope these helphttp://soliforum.com/i/?p8HgXxI.jpghttp://soliforum.com/i/?OHIjrw2.jpghttp://soliforum.com/i/?5V4G2fD.jpghttp://soliforum.com/i/?rpga7sG.jpg

4 (edited by The Plasticator 2021-04-05 19:22:38)

Re: Distance between filastruder & filawinder

When pulling the filament over to put in the Filawinder it takes lots of trial and error.
I let the filament get about table height and gently grab the end and very slowly, as the filament extrudes, Drag my hand across the table until I get enough to thread into the winder tube.
I keep a pair of wire cutters close because I often have to trim some hoopties or not very strait sections off.
If you try to feed a really kinky piece in the tube it may hang up so be patient getting it started.
It is a challenge but you learn how to do it, but I have not gotten real good yet.

Also I put a small strip of duct tape on the feed tube so if you get a few not bad waves they won't pull your feed tube out of the holder.

If you look in the introductions section of the forum I have posted some simple mods that worked pretty well.

5

Re: Distance between filastruder & filawinder

One other thing is be sure to put a second nut on the Filawinder spool thread rod.
I had mine loosen up and stop feeding.

6

Re: Distance between filastruder & filawinder

Started a new run tonight.http://soliforum.com/i/?YZaiF3U.jpghttp://soliforum.com/i/?e8MhMyu.jpghttp://soliforum.com/i/?J8vXR96.jpg

7

Re: Distance between filastruder & filawinder

Thank you all for your answers.

I separated a little over a meter and it works perfectly.

Thank you very much.