I have a homemade extruder that has worked perfect for ABS. Excellent diameter tolerances and speed.
2 heatzones separately controlled by PID controller. 20mm diameter barrel and 20mm auger. Total lenght of barrel+heaterzones is about 20cm.
Auger run by a 1/4hp motor controlled with a variable frequency drive with TOTAL control of motorspeed regardless of load.
But as i have moved on to PLA problems came quick.
I run vertical, and have tried 45degree tilting, but filament comes out all between 2.20-2.8 no matter what i do.
It goes in constant waves at about 1-1.5m.
Cooled by a big 120mm fan, just right at the nozzle. I have tried ducting airflow, no ducting, one 120mm fan and two 60mm
fans direct after the big and coiling to the floor. No difference.
I have a homemade winder that goes on/off controlled from a readingfork the filament goes through. Thought first that it was becuase the on/off'ing of motor and swinging filament , but coiling to the floor is the same.
Predrying PLA for 4-5hours in oven, tried both with and without PLA colorant.
Different speeds and temps but the same waving in diameter, just different lenghts. Always consistent waving.
Read a hint that auger perhaps too far from nozzle so i tried an auger that was longer (end 3-5mm from nozzle)(previous auger ended 30mm from nozzle) no difference.
Tried cutting auger at 45 degree angle at the tip (previous 90 degrees(straight cut)) no difference.
There is ONE thing i think is the cause of my problem, but i am not 100% sure.
If i take off the nozzle and run the extruder i can see that the molten plastic is slowly pulsating out from the heater.
I am not sure WHY it does so, and if this could be my problem (varying pressure?) or how to fix it.
Or do i have too short barrel?
Anybody have any tips? Or am i the only one who have experinced this?
I don't want to give up because i like to print with PLA much more than ABS.