1

Topic: Calibration nut turns with screw

I'm trying to calibrate my AiO printer, but the A screw isn't affecting the bed at all.  I looked and see that the nut is turning with the screw.  Does anyone know how to fix that?

utube / watch?v=S-9TQMn9qKQ

Thanks

2

Re: Calibration nut turns with screw

dmcgauley wrote:

I'm trying to calibrate my AiO printer, but the A screw isn't affecting the bed at all.  I looked and see that the nut is turning with the screw.  Does anyone know how to fix that?

utube / watch?v=S-9TQMn9qKQ

Thanks

I had this issue on my 1.0. You will need to take the bed apart and glue the nuts in place with super glue. Careful not to get any in the threads. The plastic housing around the nuts strip easily.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

3

Re: Calibration nut turns with screw

Awesome, thanks!