Topic: Trying to print gears
I've been trying to print the Botmobile gears (ABS) unsuccessfully on my new 1.0 printer. They seemed to print decently on my 2.0, but not this one.
I've tried the xyz filament and my Hatchbox filament. I originally printed the hatchbox gears at 215/70 on my Duo.
As you can (hopefully) see the gears have bowed in the middle.
Unfortunately I have the new 1.0A version, and cannot use repetier, and xyzmod software is broken, so i have no choice but to use the stock software.
i am printing at 90%, .1mm, slow speed. The temp default to 215/90. I've tried fast speed, .2mm resolution, raft, no-raft.
I tried to print with a hairdryer set to low inside the enclosure in hopes to limit the cooling and contraction of the part. It helped abit, but not enough.
Does anyone have any idea how I can print these successfully?
The pictures show the red XYZ filament.
Ignore the raft: