Just spray the bottom of the glass with hairspray and set it on the aluminum plate with or without the Kapton tape in place. Then heat/cool 3 times and it'll stick yet still be removable without the warping and other issues caused by binder clips.
Printit Industries Model 8.10 fully enclosed CoreXY, Chamber heat
3-SD3's & a Workbench all fully enclosed, RH-Slic3r Win7pro, E3D V6, Volcano & Cyclops Hot End
SSR/500W AC Heated Glass Bed, Linear bearings on SS rods. Direct Drive Y-axis, BulldogXL
Thanks to all for your contributions