Topic: cheap Octave Kaptan tape 100' rolls warning

it may be only $15 a roll but its so much thinner and low quality than what comes on printers that nearly each print tares of pieces even if you just pull print loose after cooled. so its 'Cheap' on many levels just not on fewer replacements needing applied which is a real PITA also. as all standard methods of applying it dont work as they should.

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs