Topic: Calibration and Extruder to Bed Clearance Questions & Discussion
I am extremely new to the 3d printing world and I purchased a davinci 2.0 for my first printer. I have been doing some reading and tinkering with the printer but I am still confused about a couple things. When you use the auto calibrate ( mine seems to work fine) and you set it to a z-offset for all 3 points of say 125mm, does this directly affect how close the print head is to the bed on the first layer?
Since I have messed with this it almost seems like my print head is too close to the bed, but I thought that would be in the print file itself and the calibration is just for level?
Also I remember seeing a picture description / guide of what a print looks like with the print head is too close and too far, anyone have a link to that?