Topic: never call her `honey`
one of my previous work... 11 cm (4.5 inch) tall
a tricky print
you will need support and brim (or raft)
this one was sliced with Kissslicer with :
layer_thickness_mm = 0.2
skin_thickness_mm = 1
2 perimeters (loop)
support set to medium and 45°
then the gcode was used in Repetier with the feedrate slider around 70% of the speed (with little details like the axes, low speed is better )
heat bed set to 95°C
head set to 195°C
i used green `glow in the dark` for this case.. (lot of this filament, and no more white in stock
)
ang glass bed with kapton
you can download the stl here : http://78ps4n.1fichier.com/ (too big for the forum, just click on : telecharger le fichier button)
the gcode here : http://lj6uev.1fichier.com/