Topic: Oven baking old ABS

I was having some trouble with good prints.  I could also hear some crackling when extruding.  The picture below is extrusion before and after 2hrs of baking at 170F.

http://virtualvector.com/wp-content/uploads/2014/09/ScreenHunter_07-Sep.-14-16.21.jpg

You can see it made a significant change in the quality of what is coming out of the nozzle and what a little bit of moisture can do sad