Topic: pig character iphone case
a friend ask me to do a pig character case she saw on the internet, so i just got the stl model from thinkverse, and add the ears, and model the different parts in autodesk maya... first print was no good as i forgot to level(?) the ears and the result was not pretty, at the second try the result was nice but i broke the piece in the middle ..third time was the charm and most pieces came out right at first print, but the eyes,,, just to small to print and handle, so i just improvise with a hair clip(?) sand the case and the parts and super glue all... not as nice as plastic injected stuff, but close enough, she walk away happy... lesson learned... ABS cracks soo easily and little pieces are really hard to post treat (sand, heat and glue) ...
thanks for any comments
Cheers!