1 (edited by LdyMox 2014-08-13 18:16:42)

Topic: Bronzefill

Ok I was posting a lot of my prints in the new Colorfabb Bronzefill (90% bronzepowerder by weight)  in the post below. But since I am just posting prints now I am moving to here unless it's new information about the material or processess

http://www.soliforum.com/topic/7012/col … ronzefill/

D10 dice, printed solid and no numbers. I plan to paint/magic marker the numbers on later. Ok not too exciting. lol

http://www.soliforum.com/misc.php?action=pun_attachment&item=5967&download=0

Post's attachments

20140812_203416-1.jpg 1.79 mb, file has never been downloaded. 

You don't have the permssions to download the attachments of this post.
Tammy
Solidoodle 2
E3Dv6 Hotend, MK5 v6 version, Glass Bed, Anti Z backlash slop nut, SureStepr SD8825 1/32 Extruder Driver, makeshift breakaway plexiglass case; . L-Cheapo 3.8 Watt Laser Attachment w/Custom built enclosure
From Buffalo, NY, USA

2

Re: Bronzefill

Could be cool to get a set of metal number punches from ebay or the hardware store, heat them up a bit in the oven and use them (via a pair of pliers) to melt-press the numbers into the outside...

SD3. Mk2b + glass, heated enclosure, GT2 belts, direct drive y shaft, linear bearings, bowden-feed E3D v5 w/ 0.9° stepper
Smoothieboard via Octoprint on RPi

3

Re: Bronzefill

grob wrote:

Could be cool to get a set of metal number punches from ebay or the hardware store, heat them up a bit in the oven and use them (via a pair of pliers) to melt-press the numbers into the outside...

Great idea, something like these Harbor Freight eighth-inch stamps could work nicely!

Don: Folger Tech 2020 Kossel Rev A + Borosilicate + Snow Effector
        Davinci 1.0 + Repetier : Filastruder
        SD3 + RAMPS + Lawsy Carriages + E3D + Borosilicate + ... : Cupcake

4

Re: Bronzefill

Yup, that's what I was thinking of...

SD3. Mk2b + glass, heated enclosure, GT2 belts, direct drive y shaft, linear bearings, bowden-feed E3D v5 w/ 0.9° stepper
Smoothieboard via Octoprint on RPi

5

Re: Bronzefill

Oh that's a great idea. And I don't think it would mess with the weighting too much.