So today I made a run to Lowes and picked up an 8inx8in piece of polycarbonate (Lexan) and an 8in x 8in piece of acrylic.
First off it looks AWESOME. Second, I have never had a build platform that let things adhere this easily.
Heres what I have found so far!
Poly/Lexan
Pro's:
Amazing Adhesion with no form of glue, hairspray, and very little to no heat.
Looks Cool
Parts pop off w a little cold compressed air
Cons:
Bends up just a wee bit with heat but im testing how low I can go with the heat and still have it stick. Even with it bending up I just use a couple binder clips and I have 0 issues.
And now for the Acrylic!
Oh wait I havent tested it yet. Ill update when I get to it!