Topic: Rough prints... Help Please
Good evening folks....
Just wanted to stop in and ask for some info on rough prints...
I recently got my SD3 back up and running correctly... but am having some
issues with rough prints and wanted to share a couple pics and some
info and see if you guys could help me diagnose the issue...
First... I have included 2 images. First, shows the outside walls of the project
I am printing... and you can see the rough corners of the walls. Not nearly as smooth
a surface as I would expect. Second, is a pic of my infill which looks kinda sloppy to me
as they are not nice and neat layers....
What I have done today....
1. Adjusted tension of belts (which now seem to be correct)
2. used lithium grease and lubed all rods and bearings... (had a intermittent squeak that was bothering me)
3. Flow rate adjustment (did this, and my first box wall measured .52 and after adjust and another box print, I got .43 wall thickness)
Like wise I currently have these settings in Slic3r:
Speed:
perimeters: 75
small perimeters: 55
External perimeters: 60
and layer heights at: .2
so... what could be the issue here???? any suggestions????
Thanks for the help!