Topic: Firmware, Clacking, Eeprom, Oh My!
Does the Marlin beta firmware change the eeprom layout or perhaps allocate new fields or reinterpret old fields that have bad random values leftover from the original printrboard firmware?
My just completed experiments sure seem to indicate something is screwy:
http://home.comcast.net/~tomhorsley/har … mware.html
Test cubes made clacking noises on retraction and didn't print well till I put back the original flash and eeprom I saved off before starting the experiment.