New at this. Pictures are of a print that should have flat tabs to use for attaching with screws to flat surface.
This is try #2, with speed slowed down, extra sticky and so on.
ABS at 245C and bed at 60C (first layer at 70C)
The print was started very well, with quite a few layers, perfectly flat.
Apparently, no matter what i do, the tabs will peel themselves up at some point.
I think the large ring they are attached to is shrinking due to cooling, more than the bottom most layer,
and hence it pulls up the tabs.
Is this a well known problem?
Are there workarounds with design change or temperature settings or such?