Topic: Silver faery pendant
i just receive a real print from shapeway of a pendant i made for my wife.
it was made in glossy silver : cost around 100$ (with taxes and shipping)
i'm happy.. my wife is happy ![]()
sorry but this time, i sells the design if you want one...
EDIT : i forgot to say that all donators that made a donation of 20$ or more can have this design for free. Just send me a Pm/email with the name you used for the donation and i will send you the file for free.
This offer will ended the 1th september 2013