Topic: Heated platform during print?
Do i need to have the platform heated during whole print?
//Matte
You are not logged in. Please login or register.
SoliForum - 3D Printing Community → Solidoodle Discussion → Heated platform during print?
Do i need to have the platform heated during whole print?
//Matte
Yep... if the bed drops below 60c and you're using ABS, the print is likely to pop off the plate. Keep it at the 70-80c range to insure the print sticks.
Ok , thanks ![]()
//Matte