Topic: Wood filament
I wanted to create a metallic material ended up with this


You are not logged in. Please login or register.
SoliForum - 3D Printing Community → DIY Filament Materials → Wood filament
I wanted to create a metallic material ended up with this


I wanted to create a metallic material ended up with this
You should checkout Protopasta. They make filaments that have metal powders in them and can even be polished like the real metal once printed. They have copper, steel, I believe bronze is even available.
wanted to make sth metallic ended up with a wood-like material as you see in the pics...ABS pellets with gold metallic paint
more pics here : https://www.sk3tchup.com/2018/12/diy-ch … usion.html