Topic: xyz with repetier, bad print quality
Hi,
I recently flashed my davinci 1.0 and installed repetier firmware. I have been playing with it for some time now, but I still won't print well at all. I've got it to stick to the bed, but after 3-4 layers it comes up. I am using hair spray and the bed temp right now is about 100c. Before it "peels off" the bed, the print quality looks atrocious. It seems there is too much filament being extruded and and it creates little bumps with the zig zag pattern in the first few layers. I believe there is a setting to change that, but I not completely sure. I also tried printing with cura and without the repetier host. I get the same quality with that.
P.s. I included most settings even though they may be irrelevent
layers and perimeters
Layer height: .3
first layer height: .3
perimeters: 3
solid layers, Top: 3, Bottom: 2
//
infill
fill density 10%
combine infill every: 1 layer
solid infill every: 0
fill angle: 45
solid infill threshold area: 70
//
skirt and brim
loops: 1
distance from object 6
skirt height: 1
minimum extrusion length: 10
brim width: 2
//
support
overhang threshold: 0 (auto detect)
enforce support for the first: 0 layers
raft layers: 0
contact Z distance: .2
pattern spacing: 3
pattern angle: 0
interface layers: 2
interface pattern spacing: 0
//
speed
perimeters: 40 mm
small perimeters: 70%
External perimeters: 70%
Infill: 60 mm
solid infill: 75%
Top solid infill: 50%
support material: 20 mm
Bridges: 10 mm
Gap fill: 10 mm
Travel: 175 mm
first layer speed: 40%
max print speed: 80 mm
////
filament settings
//
Diameter: 1.75
extrusion multiplier: 0.9
Extruder: 215c
Bed: 110
//
Cooling
Fan speed, Min: 35 Max 100
Bridges fan speed: 100
Disable fan for the first 3 layers
enable fan if layer print time is below: 60 seconds
slow down if layer print time is below 5 seconds
Min print speed: 10 mm