Topic: ctc printer platform

platform heat reads out 130c, selected 110c, platform doesn't heat up, progress bar near the end and just blinks will not go further?????

2

Re: ctc printer platform

If you are reading 130c at room temp, then your thermocouples could be shorted or not connected. Also unless you set it to heat higher than its current temp it would not heat, so it is acting as it should in regards to not heating.