1 (edited by dubbsd 2016-03-06 15:37:32)

Topic: having touble with print (any suggestions)

this is the tower of PI thingverse thing:271769
as you can see by the pic second row not all the numbers printed.
I am using a Makerbot 2X , .4mm nozzle, .2mm layer thickness 2 shells
print speed of 70 mm/s what di i need to do to get it to print correctly.

Thanks

http://soliforum.com/i/?GJJqnh0.jpg

Ultimaker S3.

2

Re: having touble with print (any suggestions)

that is not an easy print to do.

looks to me like it tried to print them, but maybe broke them out as it built up?

slowing things down may help a little.

SD4 #1 & #2 - Lawsy carriages, E3D v6, Rumba controller board, mirror bed plate, X motor fan, upgraded PSU & Mica bed heater
SD4 #3 - in the works ~ Folgertech FT-5, rev 1
Printit Industries Beta Tester - Horizon H1

3

Re: having touble with print (any suggestions)

I agree with Heartless. If you look you can actually see part of the missing number merged with the next number. You might want to slow it down, or raise your print temp 5 degrees to get better layer adhesion. also make sure your alignments and heights in your mechanical structure is all good and the print head is not dragging on previously printed areas.

The X2 is a dual head if I remember right. You do not want both heads at the exact same height. Which ever head is your primary should be left where it is but the secondary head should be raised so it is about .02 to .05mm higher than the primary. If it is not done this way the secondary head will drag across previously printed layers and could knock them loose or worse knock the entire model loose.

Printing since 2009 and still love it!
Anycubic 4MAX best $225 ever invested.
Voxelabs Proxima SLA. 6 inch 2k Mono LCD.
Anycubic Predator, massive Delta machine. 450 x 370 print envelope.

4 (edited by n2ri 2016-03-12 04:57:41)

Re: having touble with print (any suggestions)

also use ABS, as PLA stays soft too long. and if slicing with Slic3r check the avoid crossing perimeters option so it dont drag over stuff as much and set a Z lift number. these add print time but save failed prints better

Solidoodle 2 with Deluxe kit cover & glass bed with heater. and 2nd board SD2 used not 3rd and alum platform not installed yet still wood. also need cooling fan installed to board. use Repetier Host couple vers. Slic3r also have all free ware STL programs

5

Re: having touble with print (any suggestions)

Thanks
I slowed the speed down to about 40mm/s and here is how it came out.

http://soliforum.com/i/?T4GYJrp.jpg

Ultimaker S3.

6

Re: having touble with print (any suggestions)

3/14/16
3.1416 rounded Pi day

7

Re: having touble with print (any suggestions)

square pie is called Cobbler ;^P